Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Soric SF or 3D CORE PET ?
Soric SF or 3D CORE PET ?
Post Reply
Like
10
Soric SF or 3D CORE PET ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Qumec
Qumec
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 77
Hi Hanaldo
Tanks for your awnser
Here is a pic of the part
Weight is not a Big problem for me what I want is the stiffness
Edited
12 Years Ago by
Qumec
Reply
Like
9
Hanaldo
Hanaldo
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Take your pick really. I wasn't quite sure what part you're looking at making, but Soric is definitely the way to go if you've got a complex shape. The PET core can flex into shapes, but not so easy. It's more flexible rather than drape-able, compared to the Soric which is more like a heavy cloth. To be honest, I was left less than impressed with the thicker PET cores, but I also don't want to conclude that they are as poor as my crude testing found.
Looking at your lay-ups, I think the PET core will be the better solution in terms of weight.
Reply
Like
8
Qumec
Qumec
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 77
Hallo ;-)
I am making Robot arms in composite and have until now Normal closed cell foam in 10 mm as core.
But my parts has shape as a tube and is made at one time, not to parts glued together, the part is a free form shape with many round shapes, so now I want to use a core material there is more easy to form and better for infusion.
Here is a link to se the parts
http://youtu.be/8PXKaC6_uJY
The Black parts is Carbon but alittle dusty :-)
But what is best ?
A)
Layer 1 : 600g Carbon
Layer 2 : Soric SF 3mm
Layer 3 : 600g Carbon
Layer 4 : Soric SF 3mm
Layer 5 : 600g Carbon
Or
B)
Layer 1 : 600g Carbon
Layer 2 : 600g Carbon
Layer 3 : 3D CORE PET 10mm
Layer 4 : 600g Carbon
Layer 5 : 600g Carbon
Tags
3D CORE PET
core materials
soric
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search