Which is stiffer pultruded or roll wrapped tube?


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Agreed.

Ultimately the pultruded tubes have all thier fibres in one direction hence slight superior stiffness down thier length.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Pultruded as long as there is no torque or bending loads
tnr0007
tnr0007
Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)
Group: Forum Members
Posts: 2, Visits: 16
Tube is in tension.