Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
mould section joins
mould section joins
Post Reply
Like
3
Prev
1
2
Jump To Page
mould section joins
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Ian974
Ian974
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 92
Not managed to get any other photos yet,been a few other jobs I've needed to get done on the car.
If I'm understanding correctly, id be looking at smoothing off the gaps with the wax/ plasticine, lay a strip of fibreglass along the join, then lay up the carbon fibre etc?
Reply
Like
3
Fasta
Fasta
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Ian974 (19/07/2014)
Not managed to get any other photos yet,been a few other jobs I've needed to get done on the car.
If I'm understanding correctly, id be looking at smoothing off the gaps with the wax/ plasticine, lay a strip of fibreglass along the join, then lay up the carbon fibre etc?
That's right. If you have to?
Fastacraft Facebook page
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search