lofty
lofty
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 14
I have some old door trims and I plan to use the backing cardboard to produce a mould - as a noob it's the first ever mold
. I'd appreciate advice for surface prep. The surface has a cross-hatch pattern like masonite. I plan to sand back and possible use a spray filler and sealer but would like advice. Tips and suggestions?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Preparing door trims for a mould
lofty
-
11 Years Ago
Don't take this as a recommendation as I am a beginner to but this is a mould I made recently. The...
Alibro
-
11 Years Ago
Spray with high build, then flat it down with 400. Then spray with PVA, nice and thick so your part...
Hanaldo
-
11 Years Ago
In my experience of working with the brown Masonite I found that body filler and glues etc do not...
Fasta
-
11 Years Ago
Is it actually masonite? I took it as just having a surface texture like masonite... If it's...
Hanaldo
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search