Can't get peel ply off cf part...
Can't get peel ply off cf part...
Post Reply
Like
3
Can't get peel ply off cf part...
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
BlackNDecker
BlackNDecker
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 92,
Visits: 251
What am I doing wrong? Quick vacuum bagging test to see where bridging would occur...
But I can't get the peel ply of the back. Should I over lap the peel ply a couple centimeters past the cf?
I followed the directions on the Easycomposites tutorial. My lay up process was:
1. 200 g cf x 3 layers
2. Peel ply
3. Infusion mesh
4. Spiral tubing
5. Vacuum bag
Any help would be appreciated. Thanks!
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Can't get peel ply off cf part...
BlackNDecker
-
12 Years Ago
Damn...this was way too hard. Is there a trick to make it easier?...
BlackNDecker
-
12 Years Ago
Been there and done that. It is so hard to remove that I was actually injuring my self with over...
fgayford
-
12 Years Ago
Yeh peel ply is a prick to remove on parts after its wet out. Best thing to do is to put release...
Hanaldo
-
12 Years Ago
You can use perforated release film between the peel ply and mesh, the peel ply can still be...
carbonfibreworks
-
12 Years Ago
I recently started using a product called infuply 2. It's a flow medium glued on to perforated...
ajb100
-
12 Years Ago
Available here .
FLD
-
12 Years Ago
I've read a lot about that perforated film above the peelply. The thing I dont get is: doenst the...
matthieutje65
-
12 Years Ago
No not at all. I always use perforated release film and peel ply in my infusions, because it both...
Hanaldo
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search