Hey all,

Thought I'd post up one of the projects I'm working on at the moment; moulding a replica Nissan Skyline R34 GTR rear wing. I have just completed the moulds for the wing stands, and a couple of reasons I wanted to post this one up was firstly because it was actually a more complex shape than it first appears, with several sneaky undercuts. And secondly, I wanted to show the way I prep my plugs.

I do not like using 2k paints, I refuse to use them myself. Instead, I spray my plugs with ordinary single pack high build primer, which I then flat down with 400 grit and go through the grades to 2000 grit before polishing up, as per normal. The high build doesn't polish up to a nice gloss very well, but I do it for the sake of surface porosity. I then spray the plugs with PVA (no wax), spraying it as I would a paint, although the PVA is actually more forgiving. This gives me a very nice, smooth, glossy surface. I know a lot of people recommend using 2k paints, and a lot of people don't like PVA. And while I see the benefits of 2k paints etc. for me, the single pack high build is a hell of a lot cheaper, a hell of a lot easier to use, and a hell of a lot safer. Then the PVA gives me very close to a perfect surface finish, and only requires a quick flat back and polish up which I do on all my moulds anyway. 

Some pictures:

https://fbcdn-sphotos-c-a.akamaihd.net/hphotos-ak-xfp1/t1.0-9/10374031_490210211110400_3271625748854312251_n.jpg


https://scontent-b-sin.xx.fbcdn.net/hphotos-xfp1/t1.0-9/10354998_490210227777065_6126143779541664383_n.jpg


https://scontent-b-sin.xx.fbcdn.net/hphotos-xpa1/t1.0-9/10447073_490210264443728_1115413107603415495_n.jpg




https://fbcdn-sphotos-d-a.akamaihd.net/hphotos-ak-xpa1/t1.0-9/1384326_490210277777060_5580091256107574179_n.jpg




https://fbcdn-sphotos-b-a.akamaihd.net/hphotos-ak-xap1/t1.0-9/10451170_497158903748864_3724049144514074959_n.jpg


Fresh off the plug, not yet polished:

https://fbcdn-sphotos-h-a.akamaihd.net/hphotos-ak-xpf1/t1.0-9/10376991_497158937082194_409693788167241882_n.jpg


https://fbcdn-sphotos-g-a.akamaihd.net/hphotos-ak-xpa1/t1.0-9/10461998_497158980415523_1647845991837888656_n.jpg


https://scontent-a-sin.xx.fbcdn.net/hphotos-xpf1/t1.0-9/10464367_497159010415520_2688770380897650311_n.jpg








Will post up pictures once I have infused a part.