Carbon exhaust pipes?


Author
Message
mwr2452
mwr2452
Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)
Group: Forum Members
Posts: 15, Visits: 28
If you stand by merit alone, there's no reason why a carbon tip wouldn't work. The tips don't get above 150C, so it's safe for the resin and fabric.
pk_090
pk_090
Supreme Being (409 reputation)Supreme Being (409 reputation)Supreme Being (409 reputation)Supreme Being (409 reputation)Supreme Being (409 reputation)Supreme Being (409 reputation)Supreme Being (409 reputation)Supreme Being (409 reputation)Supreme Being (409 reputation)
Group: Forum Members
Posts: 47, Visits: 169
Red bull exhaust pipes are made from a resin, no CF resin only.
Alex
steveastroUK
steveastroUK
Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)
Group: Forum Members
Posts: 21, Visits: 78
The very, very end of the tailpipe ? Maybe, but as everyone has noted, CF doesn't handle the kinds of temperatures you find higher in the exhaust system. Headers glow red very easily.

Steve
neilb
neilb
Supreme Being (802 reputation)Supreme Being (802 reputation)Supreme Being (802 reputation)Supreme Being (802 reputation)Supreme Being (802 reputation)Supreme Being (802 reputation)Supreme Being (802 reputation)Supreme Being (802 reputation)Supreme Being (802 reputation)
Group: Forum Members
Posts: 107, Visits: 504
maximum EGT's would be around 900-925 deg c in the cylinder
baja_patient
baja_patient
Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
To my knowledge, nobody makes headers out of CF. It may be technically possible, yet not realistic. In high HP operations with high rpms, steel headers can glow red hot without much trouble. The headers are usually steel, titanium or some other alloy. Further down the exhaust pipe, carbon could be used I suppose.

cheers
prsw
prsw
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 112, Visits: 1K
If you are thinking about the headers and all you have to find some very special and expensive resin,
and set your mind on failure.
To my knowledge this has not been done, due to the fact that titanium etc is better suited for this.


http://motoform.blogspot.se

383
383
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 28, Visits: 99
Is it possible to make exhaust pipes from carbon and have them last under the extreme heat cycles?

Would they eventually break down from the exhaust/gas?

What would be the best process to do something like this? I'm thinking custom shaped foam core "pipe" then wrap with carbon and dissolve after.

Has this ever been done on a diy basis or at all for that matter?