Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Reinforcing Plastic Motorcycle Seat Pan with Composites
Reinforcing Plastic Motorcycle Seat Pan with Composites
Post Reply
Like
3
Reinforcing Plastic Motorcycle Seat Pan with Composites
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Cornelius
Cornelius
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 3
My motorcycle seat pan bows when sat upon and I am going to reupholster it and want the plastic pant to be as stiff as possible. Originally I thought of using the pan as a mold, adding a release agent, and using vinyl ester with a few layers of biaxial, for strength and a final 2 layers of carbon fiber 12k plain weave for finish.
If that makes sense, would it also make sense to skip the release agent and just bond biaxial directly to the plastics with the vinyl ester and add 1 layer of 12k plain weave to the top for looks? Is there a problem using the existing plastic base in the new design? After all I just wanted to reinforce what is already there.
Any other ideas would be appreciated, I want to avoid the bowing of the plastic pan at all costs.
Thanks
Tags
reinforcing plastic
vinyl ester plastic
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Reinforcing Plastic Motorcycle Seat Pan with Composites
Cornelius
-
12 Years Ago
Depends what sort of plastic it's made from. Not a lot of resins will stick to many plastics, so it...
Hanaldo
-
12 Years Ago
Losing some weight would stop the seat bowing! :P Are you going to see the too side?...
ajb100
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search