Hi guys,

I'm going to make a Carbon Fiber replica of a Keeper helmet 

http://www.talkcomposites.com/Uploads/Images/c5b69ec7-3b1b-4cfd-b0a3-cad0.JPGhttp://www.talkcomposites.com/Uploads/Images/853f1957-7024-4864-80fd-4160.JPGhttp://www.talkcomposites.com/Uploads/Images/0408d9dc-60d8-47e3-afcc-ea0f.JPG
It will be a Gelcoated mould and so on...thats not the problem I have...

The problem is:

The helmet I have now is made from PE (I guess it's just thermoformed)
I will need some carbon fiber and reinforcement but I don't really know what Lay-up I will need?
how many sheets of Carbon fiber, Fiberglass inbetween, some core, special resin,...

the helmet I have now weighs around 700grams
I want to make sure the helmet is stong enough so my goalkeeper won't get hurt :p 

If i'm not clear enough or if you have more questions please ask and I'll answer them as fast as possible!

kind regards Matthieu Libeert




Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi,

Ok so all my projects went well untill now, but now I'm having some trouble with this gelcoat :p

The first time it didn't cure...Ermm

Now the gelcoat broke after I had to force it a bit to get my part out of the mould...(had to hammer it out of the mould Smile )
Some part of gelcoat still on the mould, some are on the part...

The mould was waxed over 7 times with mouldrelease so shouldn't be a problem.

Is there in any way a possibility that Epoxy gelcoat is not compatible with a vinylester mould?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
matthieutje65 - 14 Years Ago
Paul (Staff) - 14 Years Ago
matthieutje65 - 14 Years Ago
Matt (Staff) - 14 Years Ago
matthieutje65 - 14 Years Ago
matthieutje65 - 14 Years Ago
matthieutje65 - 14 Years Ago
Joe - 14 Years Ago
matthieutje65 - 14 Years Ago
Leon - 14 Years Ago
matthieutje65 - 14 Years Ago
Manu - 14 Years Ago
Joe - 14 Years Ago
matthieutje65 - 14 Years Ago
matthieutje65 - 14 Years Ago
Warren - 14 Years Ago
matthieutje65 - 14 Years Ago
Matt (Staff) - 14 Years Ago
matthieutje65 - 14 Years Ago
matthieutje65 - 14 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search