I agree with whats been said.  Pigment dispersions are pre-mixed meaning you will have a much easier time getting an even colour.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
As Hanaldo says you really need a dedicated epoxy pigment. With powder it can be difficult to get an even mix once added to the epoxy leaving a slightly streaky effect to the cured part. Also because of the extra mixing you have more chance of introducing air into the resin. With pigments the solids are pre mixed by the manufacturer with resin make mixing much easier. The % needed can vary depending on the manufacturer. With West & Senior it's 5-10% by weight.

Warren

Carbon Copies Ltd
Edited 11 Years Ago by wozza
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You need an epoxy pigment. Mix in a very small amount, ie. 1-2%. 
jonoj
jonoj
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 2
Hello,

I would like to know what is the best way to colour the epoxy resin that I will be using to make a table top?

I have powder that I would stir into the mixture and the mix it in and then pour in my cavity.

Just wanted to check if that really is the best way as I read adding liquid dye can sometimes disturb the curing process.

Any comments would be appreciated.

Cheers
J
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search