Polypropylene sheet as mould material


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You dont need to as such.  For good cosmetic finish sheets i would avoid it as any flaw or uneveness in the release coat application may show up on the sheet.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
flooddylan
flooddylan
Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)
Group: Forum Members
Posts: 9, Visits: 51
Hi Warren,

Would you advise to use a release agent on pure polypropylene even though it won't stick?

Many thanks Jess
flooddylan
flooddylan
Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)
Group: Forum Members
Posts: 9, Visits: 51
Thanks both. Very helpful. Jess
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Polypropylene sheet is great for making a few flat/curved sheets.  Ensure it is pure polypropylene and not coated.  Epoxy does not stick to pure polypropylene.

You will find compared to glass that it quickly picks up scratches and dulls, so take good care of it if you need to make a few sheets.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ChrisR
ChrisR
Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
It should be OK but do a test first. I use acrylic sheet for smooth double curvature projects, just well supported on a jig and I personally use TR104 hi-temp wax which has released perfectly so far.
flooddylan
flooddylan
Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)
Group: Forum Members
Posts: 9, Visits: 51
Hi,

Do you foresee problems if I use a sheet of polypropylene (smooth, no texture) as surface for wet-lay sheets approx 1.2 x 1m?

I have been told glass is ideal for this (thank you Wozza!) but I want to create a shallow curve in the sheet.

I can test on a smaller scale but I'm not sure what might happen on this larger scale regarding release, reactions and warping?

Many thanks for your advice.