Motorcycle race seat and tank


Author
Message
Jacopo Carbonio
Jacopo Carbonio
Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)
Group: Forum Members
Posts: 43, Visits: 109
Great result! Did you used Tankerite? 
carbonfibreworks
carbonfibreworks
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
20_rc51_00 (30/03/2014)
looks great!

infusion or prepreg?

what did you do to solve the tank vent issue? both for pressure and vacuum?

Also how about the issue with ethanol deterioration? Perhaps they have access to etoh free race fuels?!


I used infusion and the cap is vented so that saved me fitting a breather pipe, the bike will use race fuel so no ethanol issues but i did seal the tank with one of Caswells products.
Regards Chris
carbon fibre works ltd 

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
20_rc51_00
20_rc51_00
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 95, Visits: 548
looks great!

infusion or prepreg?

what did you do to solve the tank vent issue? both for pressure and vacuum?

Also how about the issue with ethanol deterioration? Perhaps they have access to etoh free race fuels?!
carbonfibreworks
carbonfibreworks
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Images of the mould as promised.





http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Brian2fast
Brian2fast
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
Hi Chris

Yeah, I'd like to see your mould. It's always good to see larger, more complicated moulds.

Craig
Toffee
Toffee
Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)
Group: Forum Members
Posts: 36, Visits: 118
Great work dude  Cool
carbonfibreworks
carbonfibreworks
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
FLD (21/03/2014)
Thats awesome.  Can I ask how many hours (days) of work that took?  I always like seeing other peoples mouldings.  Knowing how much time and effort go into mine I'm kinda curious about how long other people take with theirs.  It'd tell me if I fanny about too much!




I would say around five/six days in total including mould making but then again i seem to fanny about too much also Smile 
Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
carbonfibreworks
carbonfibreworks
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Brian2fast (21/03/2014)
That looks cool as! Love it.

Any chance of a pic of the underside? Just to see how the top and bottom are joined together?

How many layers is that made up from?

Craig


Hi Craig
Sorry i did not take a pic of the underside but  i can take some images of the moulds if that helps, I used 5 layers of carbon and placed Kevlar in the stack at strategic points.
Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
FLD
FLD
Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Thats awesome.  Can I ask how many hours (days) of work that took?  I always like seeing other peoples mouldings.  Knowing how much time and effort go into mine I'm kinda curious about how long other people take with theirs.  It'd tell me if I fanny about too much!
Brian2fast
Brian2fast
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
That looks cool as! Love it.

Any chance of a pic of the underside? Just to see how the top and bottom are joined together?

How many layers is that made up from?

Craig
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search