Group: Forum Members
Posts: 363,
Visits: 3K
|
It depends on what you classify as "structural strength", by removing the core in areas you are reducing the strength in that area from a bending aspect as you are reducing the effective depth of the section, you will also reduce the stiffness/increase the deflection of that area too. BUT as mentioned, you gain a hard spot for mounting points or impact areas as you create a thicker solid laminate so better bearing and point load distribution, also by joining the upper and lower layers between the core you can increase the torsional stiffness of the part with a bit of cleaver thinking
|