Silicon carbide and graphite as additives in composites.
Silicon carbide and graphite as additives in composites.
Post Reply
Like
3
Silicon carbide and graphite as additives in composites.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
rbpatil
rbpatil
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 8
Silicon carbide and graphite are to be used as additives to epoxy matrix glass fibre composites for improving certain properties. What type and what processing is required on Silicon carbide and graphite to ensure wettability with epoxy resin. There is also an issue of density difference between epoxy resin and Silicon carbide/graphite which may cause problem in mixing. Thanks all.
Reply
Like
3
ajb100
ajb100
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
I can't comment on the addition of carborundum, but I have used graphite.
Graphite powder simply needs to be mixed/stirred in to the resin
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search