Hi Guys.

 

Looking to infuse this part. Please have a look at diagrams attached.
I had an unsuccessful first infusion other day. My setup was the standard easycomp spec of resin feed spiral wrap all along length (but not the 2 ends) vac connection opposite with the 2 layers mesh for airflow. Part covered in infusion mesh. Main issues were resin barely making it to far ends (not surprising) and resin getting to vac line way before far ends had infused (again unsurprising)

 

So my thoughts were:

 

Option 1 (Fig. A): Abit of the first method , plus the standard centre feed infusion method. I would run spiral wrap wrapped in peelply, rather than double mesh along the length and also 2 ends.

Resin feed along length but maybe stopping short (x dims?)To try keep resin away from the vac spiral and possibly into the vac line before all part is completely infused, maybe not an issue tho!

 

Option 2 (Fig.B): Same standard set up but resin feed along length and also the 2 ends, plus maybe even taping up the the wrap partially along length to ensure plenty resin gets to the far end. Plus also stopping mesh short around the vac inlet to slow down the resin feed to remedy the problems i had.


Attachments
FIG A.JPG (478 views, 37.00 KB)
Edited 11 Years Ago by brettalloy
Reply
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
I am not an expert as I have only done one CF project so far.
The neck of my harp is about 1.8m long and down to about 50mm wide in places. I infused this by putting a double layer of infusion mesh across the middle (The bit that is top left in the first picture of the link.) with spiral wrap resin feed over this. I had vacuum lines at both ends so that I could clamp them off individually when the resin got there.
I know everyone says that you should infuse across the shortest direction but infusing this from the middle out worked for me.

http://www.talkcomposites.com/8522/Harp

Brian.