i was on the easycomposites site and noticed that the unimold gelcoats are only good up to 90deg c.

i plan on doing alot of resin infusion, baking and post baking and i will need to bake up to 120deg c, what other mould making products are good at these temps?

some might say that baking at such a high temp with resin infusion is unnecessary, and yeah it kind of is but after a few months i hope to be doing pre preg with an autoclave. the supplier i have in mind for pre preg has said that temps of 120deg c are needed to adequately cure.

thanks
Cole