Use the data sheet density data to convert from weight mixing ratio to a volume one.  We don't recommend it generally as epoxies are sensitive to accurate mixing ratios and it's introducing another potential area of error.

You can get micro scales that will go down to really tiny weights if needed.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Get yourself some syringes. Makes measuring by weight an absolute breeze. I used to be happy if I could pour within 0.05 of a gram of what I was aiming for, but with a syringe I can get it spot on to 0.01 of a gram every time.
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
As Matthieu said, most materials (especially liquids) change volume with temperature, the resin and hardener may change volume at different rates so your mix ratio would be different at 17deg and 25deg. Maybe only marginal but ratio by weight is more accurate and will not change the ratio if working in different temperatures
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
As far as I know I think it is still easier to mix by weight :p might be personal.
Keep in mind that some type of resins might expand/shrink (have other viscosity) due to temperature...making it not accurate enough to do it that way.

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Boatweasel
Boatweasel
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 7
I have received a pack of resin and hardener,and the only mixing information is by weight.
It would be much more convenient to know the proportions by volume as this is much easier to 
measure for small quantities.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search