Group: Administrators
Posts: 2.5K,
Visits: 8K
|
I would perform the repair exactly as in the video. Several patches larger than the damaged area can be laid ontop. If you are worried about a ridge, you can make each patch smaller so its easier to feather the edges in when you finally sand it smooth.
Release film is good for the job and you should be able to squeeze and smooth it by hand, however some small weight wont hurt it.
Make sure you sand back the whole area the patch is going onto, both to ensure a good bond, and also to make sure there is no unseen damage.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|