So, I have a 95 winnebago T4 camper.  They have a notorious and well documented issue with cracking on the pop top ASA plastic roof.  I was prepping for a trip away and realised the crack mine has on one side opened up again

I took a 2 pronged attack.  I resealed the crack with ASA plastic rod (soldering iron to weld).
Secondly I had some 4-layer carbon fibre sheet left over that I decided to attach to give some support (mix of the profinish 210g and the twill 2/2 200g) with epoxy resin.  Wet lay on a mirror finish sheet of aluminium.  Over the length of the sheet, obviously some flex but its pretty rigid.  About 1.5mm thick measured.
I know from previous peoples attempts that bonding to ASA can be tricky but I had ET538 honeycomb bonding adhesive around so I figured I try this with the backup plan being putting a few holes/rivets through the top.
I roughed up the ASA, cleaned, put the adhesive on the CF and stuck on with gaffer tape holding in place (not easy to get a clamp on)
Left for 48 hrs and was shocked to find this:



I can't work out how this is physically possible!  the forces to do this must be huge.  Neither the CF or the ASA seem to expand much with temperature.  It clearly bonded well!  I welcome thoughts as to how this is possible.  May yet put matching on the other side but with a different adhesive.  Has it reacted to the ASA?


Replies
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
dazedproductions - 5/20/2019 6:29:55 PM
Any suggestions on what I should try adhesive wise for a second piece?  
Thinking VM100 or ET500
ET500 is a bit faster and I want to catch it in the closed up state so I lean towards that. We also now know that ET538 bonds so possibly a good sign that 500 will?

Methacrylate like plexus? 





dazedproductions
dazedproductions
Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)
Group: Forum Members
Posts: 7, Visits: 25
Fasta - 5/21/2019 5:07:05 AM
dazedproductions - 5/20/2019 6:29:55 PM
Any suggestions on what I should try adhesive wise for a second piece?  
Thinking VM100 or ET500
ET500 is a bit faster and I want to catch it in the closed up state so I lean towards that. We also now know that ET538 bonds so possibly a good sign that 500 will?

Methacrylate like plexus? 

Thanks for that.  The MA310 for use with 'Difficult to bond plastics' sounds like it might be the ticket and 30 min working strength time.