Hello, I want to buy resin that should withstand temperatures from -10 to +30 degress celzius. It will be placed underneeth roof so it will not have direct impact of sun and protected from rain. I was thinking for GlassCast 50 Clear Epoxy Casting Resin for casting and GlassCast 3 Clear Epoxy Coating Resin for coat. I just want to knov that it will not crack under this temperatures, if maybe overtime it becomes little yellow beacuse UV is not a problem.