Hi there

Im looking at making some automotive and bicycle parts and I would like to use the vari-preg system as I have a laboratory oven im converting to cure composites.
In the video you say that curing time for the prepreg is 8 hours at 80°c, for me thats a bit too long as I dont want to leave parts curing overnight, especially if i get a bag burst. 
Ive looked on the site but may be not hard enough, can the cure cycle time be reduced if the temperature is increased? and do you have to have a special ramp and dwell period during the cure if so?

Many thanks
Garry
Replies
scottracing
scottracing
Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)Supreme Being (5.5K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Hi Matt
Thanks for the info, Im used to working with prepregs in motorsport and aircraft use and everything is cured in clave,s and then usually post cured at 200+ so Im trying to figure out what i can reliably do at the workshop.

Thats great news that I can get the easy-preg material delivered to germany, Im in cologne so its not far too travel for a courier. And thanks for the cure cycle, the ovens ive bought have variable temp rate controllers so this should work out well.
One question I do have is has any one tried your mould material to 120degrees? Im hoping to use your mould material to make the first parts prior to getting some high temp epoxy block tooling machined.

Thanks
Garry
Paul (Staff)
Paul (Staff)
Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)
Group: Administrators
Posts: 134, Visits: 614

Hi Garry,

if you are referring to the Unimould system then the answer on a 120 degree cure would be yes and no! The design temperature is 80°C, at 80°C the service life of the tool will be almost indefinite, however we have on occasion pushed the tooling to °C with good results (but never higher), as you are well beyond where it is intended to be used I would be prepared to expect the moulds to degrade more quickly and potentially lose some dimensional accuracy. I very steady ramp up to the 120°C (say 10°C/hour) to post cure the mould before use would be essential to prevent the mould from off-gassing and softening whilst in contact with the prepreg.

You are in experimental and out-of-parameter territory sotry this at your own risk!  My advice would be to stick to the 8hr @ 80°C. You will probably find that with most ovens this will actually use less energy than 2hrs @ 120°C



Paul Statham
Easy Composites / Carbon Mods - Technical
Edited 12 Years Ago by Paul (Staff)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search