When trying to cut fabric carefully to make small parts, what do people use? Shears are fine for larger parts, but when I want to cut out reasonably accurate parts, I was planning on using a knife and cutting mat, but not sure if it will simply blunten the blade quickly and start ton pull the fabric?

MacG Racing Ltd., UK based Motorsport Racing Team - follow us on Twitter and on Facebook
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
I use a number of tools, a pair and small shears from EC and i also use a curved blade surgical scalpel plus one of the wheel cutters below. Make sure you have a cutting mat etc under the fabric.
macgtech
macgtech
Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)
Group: Forum Members
Posts: 20, Visits: 102
That's great, thanks Chris.

MacG Racing Ltd., UK based Motorsport Racing Team - follow us on Twitter and on Facebook
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Your welcome, you will be surprised how well the wheel cutter works Smile
Chris
www.carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
macgtech
macgtech
Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)
Group: Forum Members
Posts: 20, Visits: 102
Mat and wheel arrived this morning, so will report back when I have given it a whirl!

MacG Racing Ltd., UK based Motorsport Racing Team - follow us on Twitter and on Facebook
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search