Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Hello,
I have just bought some silicon mold making rubber and some epoxy casting resin which I would like to use to replicate some tabs on some parts I am making. The original part has locating tabs on the inside, and as I am making this part out of carbon fibre, I will need to replicate the tabs then bond them to the new part.
I have never used silicon molds or casting resin before, though it seems pretty straight forward. My issue is with the shape of the tab:
I think this should be very easy to mould, but I am forecasting issues with casting. Due to the shape, the resin is not going to stay where I intend it to stay (damn you gravity
)
. The only way I can see around it is to place the mold on it's side, then create a dam next to the mold with coreflute or something, then fill this up with resin. Is there an easier way of doing it that I am overlooking?
Thanks for any help, sorry if my explanation doesn't make much sense.
Cheers,
Martin.
Reply
Like
5
Reply
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Right, all studied up and on the same wave length! Thanks for that mate, that will work much better than what I wanted to do.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How to cast this shape?
Hanaldo
-
11 Years Ago
Build a small box around the tab using corex and secure with hot glue, make sure you have used...
carbonfibreworks
-
11 Years Ago
Hmm, don't think I expressed what I meant very well. Molding the tab should be easy, that's not a...
Hanaldo
-
11 Years Ago
Why will you have a thick part ? it will be an almost exact replica of the original tab. Chris...
carbonfibreworks
-
11 Years Ago
Ohhhh I might have just clicked onto what you mean haha. Would you replicate the WHOLE tab? So do...
Hanaldo
-
11 Years Ago
Make it as a block mould in silicone and make cut lines through the part with a scalpel to help...
carbonfibreworks
-
11 Years Ago
Right, all studied up and on the same wave length! Thanks for that mate, that will work much better...
Hanaldo
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search