If the nails rip through the cells, it is because you have not placed them far enough into the core. You need a good 4 or 5 layers of cells above the nails to stop it ripping through.
This might seem wasteful, but the sheets are deliberately a little oversized.
Your picture of the expanded honeycomb does not look that bad. A few more cells would have been a bit more even had the nail method worked successfully, but generally even with the professional machines, you still get some cell distortion.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|