Just my thoughts on seeing your project.
1) Why not make a carbon door and then bond in the OE steel frame? Yes it will be slightly heavier but it will be a lot less fragile.
2)If you want to make the frame in carbon why dissolve out the foam on your new design? Make it in PU or PVC foam and use that as a rigid core. The foam is light so the amount of weight you'll save is negligible and the strength it will add makes it worth keeping.
|