Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
making a mold out of styling clay
making a mold out of styling clay
Post Reply
Like
5
making a mold out of styling clay
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
jontex
jontex
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 4,
Visits: 91
Hello! New to the forum.
How do i make a finnished mold out of this clay?
http://carbix.se/product.html/styling-lera?category_id=25
I have made a prototype looking similar to this:
http://a248.e.akamai.net/origin-cdn.volusion.com/hddtq.vzwer/v/vspfiles/photos/13440Z-2.jpg?1348857922
What would be the next step after making the prototype? I cant wax the clay or put release agent on it to make the gelcoat release...
Should i juste throw the s*** clay away and make a prototype out of someting else?
Best of regards from Sweden, great site u have here
Tags
clay
mold
prototype
Reply
Like
5
Reply
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
The thing I would suggest you to do is use a vinyl wrapping stickersheet and put it onto the clay... its what they do, to make scale models of conceptcars...
you can 3D shape the vinyl onto the clay by using heat...after you've applied the vinyl you can just add releaseagent and gelcoat and so on.
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
making a mold out of styling clay
jontex
-
12 Years Ago
The thing I would suggest you to do is use a vinyl wrapping stickersheet and put it onto the clay......
matthieutje65
-
12 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search