| 
	Group: Forum MembersPosts: 27, 
    Visits: 39
 
 | 
                    
			            Hey Alan, 
 What temp are you working at, I had some real problems earlier in the year with cure times when I was working in my cold shed some stuff was taking days to cure. if you are getting problems with the resin draining, this could be that it's not curing fast enough so it's running off, or it could be that you are trying to build too thicker coat which is causing the runs. with your curing issue i would say that you have put it in the oven too soon, but I'm not an expert on that one. good luck with it buddy.
 
 |