			            Hi Chris,
  Yes, please post a photo and I'll be able to give you a more reliable answer. From what you're saying both could be suitable, it depends on the shape of the screen, if it curves in just one plane (which is what I'm expecting) or at least a sheet that curves in only one plane would be suitable then either of the two sheet types you mention could be used. Without seeing the photo I'm under the impression that our Thick Flexible Carbon Fibre material would be the one to go for.
  Best regards, Matt                
			            
  				