Hi everyone I like know if there is on sale some kind of elastometric resin? like the ones used on some  knife handles and grips foot holders.  a kind of a rubbery surface!

thanks! 
Reply
Warren
Warren
Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)
Group: Administrators
Posts: 214, Visits: 783
Hi Matt

which scale of shore hardness are you using?

I ask as i was looking at scales earlier and shore hardness 80 on scale A equates roughly to very hard shoe heel rubber, where as on scale D it equates to the plastics used in hard hats, so obviously there is a big difference.