Elastrometric Resins


Author
Message
kylle
kylle
Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)
Group: Forum Members
Posts: 34, Visits: 101
Hi everyone I like know if there is on sale some kind of elastometric resin? like the ones used on some  knife handles and grips foot holders.  a kind of a rubbery surface!

thanks! 
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Kylle,

Actually, yes. We're just about to stock a brand new high performance flexible epoxy resin system. It cures to an 80 shore hardness and can be used either as a laminating or a coating resin. It's a two-part mix, 100:120 ratio. It's called EF80 and we will be taking delivery on in around 7-10 days. Here's a link to it on our site:

https://www.easycomposites.co.uk/ef80-flexible-epoxy-resin

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales