As Warren says, the difficulty here is the recesses. You could use multiple pieces of profinish to achieve it, using neat cut lines around the recesses to get the neat finish, but it would be a hell of a lot of work.
Some areas would need seperate pieces of fabric with cut lines on corners to aid alignment and fabric folding. Then you would need to get the surface main layer of Pro-Finish to line up neatly.
IF you did tackle it, i would certainly be spending most of my time making accurate thin paper templates to ensure you only cut the carbon once.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|