What Warren says is correct.
Due to the difficulties already mentioned, we don't generally advise any vacuum processing of skinning at all. If the part is too hard to do skinning, then you really want to consider moulding it as it will in the long run probably save you time and expense in wasted materials.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|