I'm in the middle of my first attempt at carbon fibre laminating using the CarbonMods starter kit with the 100 to 30 ratio resin and when I apply the base coat of resin I cannot get it to keep an even coverage over the surface of the mould, it just wants to pool up at the bottom of the mould leaving dry patches on the angled faces.

Can anyone tell me what could be going wrong here? Is there anything I can do to put it right? The resin is still runny at the moment and i have tried to keep brushing it back from the bottom.
Replies
TomDesign
TomDesign
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
Photos help always a lot.
RyanParle
RyanParle
Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)
Group: Forum Members
Posts: 20, Visits: 1.2K
Sorry I cant seem to upload any images, posting this from my mobile. 
Ithink I may have got it sorted now, I waited until the resin had thickened up a little then gently brushed it back over the dodgy areas.

I'll let you know how I get on.
Edited 13 Years Ago by RyanParle
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search