They are not the most accurate guages on the market but they are very cheap and accurate enough for most purposes. Its the change in pump tone that is a more relevant indicator for resin infusion processes anyway.
A high quality oil filled calibrated guage would cost several times as much and be beneficial to very very few customers in reality.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|