Easy Composites Ltd - Product Specific Pages
»
Resin Infusion Starter Kit
»
Vacuum Gauge Precision (can't pull full vacuum)
Vacuum Gauge Precision (can't pull full vacuum)
Post Reply
Like
5
Vacuum Gauge Precision (can't pull full vacuum)
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
H4RTM4N
H4RTM4N
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 203
Hi all,
My name is Andreu and I'm new to this forum. I've just received my order from EC and I'm already trying to make my own carbon fibre parts using resin infusion.
For the first trial I wasn't concerned about the final quality of the part (a simple plate) as I only wanted to be familiar with the process. However, I noticed I couldn't reach 'full' vacuum. Instead, the vacuum gauge was stuck at -29Hg (0.98+ bar). I closed all the leaks in the vacuum bag but I kept having that remaining pressure inside. In order to be sure of that, I connected the vacuum pump to the resin catch-pot only. The hose that usually comes from the resin catch-pot was clamped so the vacuum was only made inside the catch-pot. When I pulled vacuum from the pot, I obtained the same result.
Taking into account that I live in Barcelona and my house is <100m above sea level, I wonder if my equipment is all right or not. In other words, I want to know if the the vacuum gauge is simply not representing the reality inside the bag because of its precision. I can imagine 2 possible answers to the question:
- YES, the equipment is just fine. The precision of the vacuum gauge of the resin catch-pot is somewhat near to 2mbar and that is why I obtain these 0.98bar.
- NO, there's something wrong. You should obtain -1bar (-30Hg), which in reality represents the advertised 99.995% vacuum.
Could you please help my clarify this issue?
Thank you a lot and good luck to everyone!
Regards,
Andreu
Tags
catch-pot
full vacuum
precision
vacuum gauge
Edited
12 Years Ago by
H4RTM4N
Reply
Like
5
Replies
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
As I understand it, Your at full vacuum at 29.9 HG so 29 is great!
You could suck a cat inside out with that kind of vacuum.
Fred
Reply
Like
5
H4RTM4N
H4RTM4N
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 203
Well but it's still far from the 99.995% vacuum advertised with the small vacuum pump (which means an absolute pressure of around 0.2mbar inside the bag). As of now, there is way more.
Reply
Like
5
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
H4RTM4N (19/07/2013)
Well but it's still far from the 99.995% vacuum advertised with the small vacuum pump (which means an absolute pressure of around 0.2mbar inside the bag). As of now, there is way more.
Throw out your cheap guage and buy a liquid filled professional guage and I am sure you will reach full vac.
I know because I had the same disapointment your having. The dealer came out and put his mega expensive guage on and it reached full vac instantly.
Fred
Reply
Like
5
prairiecustomcomposites
prairiecustomcomposites
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 722
Fred, what brand of gauges do you recommend? And where do you purchase them? I have a feeling I am experiencing the same issue with cheap gauges
Also, what makes a liquid filled gauge better or more accurate than a non-liquid filled gauge?
-Mike-
Reply
Like
6
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
prairiecustomcomposites (24/07/2013)
Fred, what brand of gauges do you recommend? And where do you purchase them? I have a feeling I am experiencing the same issue with cheap gauges
Also, what makes a liquid filled gauge better or more accurate than a non-liquid filled gauge?
-Mike-
Hi Mike
I think mine are airtech (off the top of my head). I think the liquid keeps the needle from sudden movements caused by vibrations.
Fred
Reply
Like
4
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
fgayford (19/07/2013)
As I understand it, Your at full vacuum at 29.9 HG so 29 is great!
You could suck a cat inside out with that kind of vacuum.
Fred
I just had to add this video after seeing your comment fred
OT:
I think 99.995% is in optimal conditions and so on... it's a number that is very hard to reach...
99% is 98% is allready more than enough for most applications
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
5
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
matthieutje65 (19/07/2013)
fgayford (19/07/2013)
As I understand it, Your at full vacuum at 29.9 HG so 29 is great!
You could suck a cat inside out with that kind of vacuum.
Fred
I just had to add this video after seeing your comment fred
OT:
I think 99.995% is in optimal conditions and so on... it's a number that is very hard to reach...
99% is 98% is allready more than enough for most applications
Matt That video is hilarious! What is that cat thinking, had tears in my eyes its so funny.
Fred
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Vacuum Gauge Precision (can't pull full vacuum)
H4RTM4N
-
12 Years Ago
As I understand it, Your at full vacuum at 29.9 HG so 29 is great! You could suck a cat inside out...
fgayford
-
12 Years Ago
Well but it's still far from the 99.995% vacuum advertised with the small vacuum pump (which means...
H4RTM4N
-
12 Years Ago
[quote][b]H4RTM4N (19/07/2013)[/b][hr]Well but it's still far from the 99.995% vacuum advertised...
fgayford
-
12 Years Ago
Fred, what brand of gauges do you recommend? And where do you purchase them? I have a feeling I am...
prairiecustomcomposites
-
12 Years Ago
[quote][b]prairiecustomcomposites (24/07/2013)[/b][hr]Fred, what brand of gauges do you recommend?...
fgayford
-
12 Years Ago
[quote][b]fgayford (19/07/2013)[/b][hr]As I understand it, Your at full vacuum at 29.9 HG so 29 is...
matthieutje65
-
12 Years Ago
[quote][b]matthieutje65 (19/07/2013)[/b][hr][quote][b]fgayford (19/07/2013)[/b][hr]As I understand...
fgayford
-
12 Years Ago
They are not the most accurate guages on the market but they are very cheap and accurate enough for...
Warren (Staff)
-
12 Years Ago
Thanks for the feedback people!
H4RTM4N
-
12 Years Ago
I think people are missing the point. Unless you are struggling to hear the tone change on the pump,...
Warren (Staff)
-
12 Years Ago
[quote][b]Warren (Staff) (24/07/2013)[/b][hr]I think people are missing the point. Unless you are...
morepower
-
12 Years Ago
I've just finished bagging an airbox cover... I usually get perfect bagging, but this time, even...
alebassa
-
12 Years Ago
An accurate guage will only tell you accurately what the leak has dropped to - which is irrelevant....
Warren (Staff)
-
12 Years Ago
Although I have found there is a difference in total vacuum pulled between two different pumps. So...
morepower
-
12 Years Ago
Thanks for the interesting feedback everyone. Warren made some valid points but I agree that there...
Matt (Staff)
-
12 Years Ago
Sorry for adding my two cents in this old thread, but I had to reply. Maybe it will help others...
brainfart
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search