3D printed nylon moulds for an RTV silicone part


Author
Message
dibbler
dibbler
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Sorry if this has been answered elsewhere (I tried searching!) but does anyone have any experience using 3D printed nylon as a mould for an RTV silicone part?

Specifically, my question is - would the nylon act as an inhibitor for addition cure RTV silicone (like this stuff)?  The specific type of nylon is PA2200, which looks like it's basically PA 12. 

I can't think of a reason why that nylon would cause problems, since it's not on the list of inhibitors, but I thought I'd check first!

Thanks in advance.

Dan
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
These cheap 3d printers do seem to be revolutionising budget rapid prototyping.

I want a cheap 3d scanner and cheap way of CAD machining moulds from tooling boards.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search