I've prepared my (sealed wood) pattern today for the Unimold system, and tomorrow will attempt to go through the process for the first time.

Would anyone like to propose the most likely scenarios that would result in a sub-standard moulding? I'd like to get this right first time...

Thanks all!Smile
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Ok, here are some of the things that can go wrong!!!!!!

Incompatible sealer used on the pattern/plug surface like unsealed body filler causing the Tooling Gelcoat to stick. Also if the sealer on the pattern/plug is still "green" then the heat generated during curing can cause it to soften causing release and surface finish issues.

Insufficient Release Agent, again difficult release.

Applying the Coupling Coat too soon. Can cause the Tooling Coat to "wrinkle"

Applying the Backing Layers too soon. Again the heat generated during curing can effect the Tooling Coat.

Demoulding too soon. The resin on the Backing Layers should have turned from cream to white.

And obviously "mechanical lock" caused by undercuts etc on the pattern/plug.

I use the Uni-Mould System all the time and if you follow the instructions/videos then all should be good.
Hope that helps and let us know how you get onSmile

Warren

Carbon Copies Ltd
LaxFriedrichs
LaxFriedrichs
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 58, Visits: 450
Thanks for taking the time to reply, Warren. It's really appreciated.

On the instructions PDF it doesn't mention considering surface tackiness, just that one should leave to cure for a minimum amount of time. 

Now if I were to wait an extended period of time between stages,( ie between the first and second gel coat, or between second gel coat and coupling coat, for example) is it an issue that the surface is no longer tacky?

Many thanks,
Adam
Edited 12 Years Ago by LaxFriedrichs
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Not really. As long as you don't leave it more than 24hrs between stages you will still get a chemical bond between the resin systems. The Gelcoat and Coupling coats will still be tacky (by tacky I mean not cured) after that time as they require the resin from the next stage to cure them, ie the Gelcoat needs the Coupling Coat and the Coupling Coat needs the the Backing Resin. They are all designed to work together. Again hope that makes sense.

Warren

Carbon Copies Ltd
LaxFriedrichs
LaxFriedrichs
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 58, Visits: 450
Thanks again, Warren.
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
No problem. I have learn't the hard wayWink So if a little bit of advice helps you avoid the pit falls that's great. For me that is one of the best things about this particular forum.Smile

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search