Hello,

I'm considering using CF X 4 layers to reinforce the location of a rudder tube's
penetration through the hull and cockpit deck on a sailboat. I'm wondering a
few things:

1) Am I kidding myself in using something I feel is superior to FG, when it will
ultimately be bonded to FG? What I mean is , I'm considering placing a circular
patch, (shapewise like a pizza with a hole in it, down over the rudder tube, covering the numerous
small cracks in the deck in the cockpit that radiate out from the rudder tube's present
location.
Q:
 The extremely short radius where the cracks
are located now: would they simply reform farther away from the rudder tube if I
use CF?
 Q:
If I continue the CF all the way to the walls of the cockpit deck, would this be a superior
plan of progres?
2) If I use CF, will it bond well to the fiberglass surface? What preparations should I
perform?

I am looking to greatly increase the strength of the rudder tube's interface with the hull
AND the cockpit floor.

Thank you for any reply/s.
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
@"knowsnada"

Did you try to email me?
Who is "wa8fly(at)copper.net?

Unsure

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)