Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Yep use MEKP and catalyse the repair gel in the same way as normal.
The only problem with tape or clingfilm type plastics is you want to ensure your repair stays proud of the gel coat level, so you can sand back to a perfectly smooth and invisible repair. (visible on mould, but not on carbon part).
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|