Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Incredible Discounted Carbon Fibre!!
Incredible Discounted Carbon Fibre!!
Post Reply
Like
8
Incredible Discounted Carbon Fibre!!
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Warren (Staff)
Warren (Staff)
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Ok guys, we have a very special deal on some very special carbon! This is the best wholesale offer we've done so far!
This incredible, 1st quality 375g 3k 8HS weave 1m wide carbon fibre has been returned from a cancelled wind-energy job. There is no evidence of any damage to any of the rolls and the carbon itself is stunning.
This 375g 8HS fibre is perfect for resin infusion (it was intended as the reinforcement for resin infused wind turbine blades) but is equally well suited to wet-layup or vacuum bagging. The 8HS (8-Harness-Satin) weave gives the fabric a really great drape-ability and at 375g/m2 the cloth is tightly woven and very uniform.
The very flat surface of this fine 3k fibre makes it suitable for surface or backing layers. As a surface layer the unusual 8HS weave certainly lends an exclusive appearance to unpainted carbon fibre parts!
As wholesale offers we are only selling this fabric in full boxes (100m) and shorter 20m rolls. At £10/m2 and £12/m2 respectively both rolls represent an incredible discount oppertunity.
This is an ideal opportunity to stock up on some carbon for your projects!!
Full details and listing:
Incredible Discount Carbon.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Tags
8hs
bargain
cheap
satin
wholesale
Edited
13 Years Ago by
Warren (Staff)
Reply
Like
8
khamon
khamon
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Awaiting Activation
Posts: 1,
Visits: 2
Warren (Staff) (26/04/2013)
Ok guys, we have a very special deal on some very special carbon! This is the best wholesale offer we've done so far!
This incredible, 1st quality 375g 3k 8HS weave 1m wide carbon fibre has been returned from a cancelled wind-energy job. There is no evidence of any damage to any of the rolls and the carbon itself is stunning.
This 375g 8HS fibre is perfect for resin infusion (it was intended as the reinforcement for resin infused wind turbine blades) but is equally well suited to wet-layup or vacuum bagging. The 8HS (8-Harness-Satin) weave gives the fabric a really great drape-ability and at 375g/m2 the cloth is tightly woven and very uniform.
The very flat surface of this fine 3k fibre makes it suitable for surface or backing layers. As a surface layer the unusual 8HS weave certainly lends an exclusive appearance to unpainted carbon fibre parts!
As wholesale offers we are only selling this fabric in full boxes (100m) and shorter 20m rolls. At £10/m2 and £12/m2 respectively both rolls represent an incredible discount oppertunity.
This is an ideal opportunity to stock up on some carbon for your projects!!
Full details and listing:
Incredible Discount Carbon.
Reply
Like
8
Dravis
Dravis
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
This was sold out some time ago... (I managed to get a 20 m roll...
) Beautiful stuff
Made some rather flash "cover-parts" for a couple of bikes.
Someone on this forum mentioned that some of the new Audi's have this "weave" as internal "decoration" panels ..
http://www.talkcomposites.com/14458/Selling--Aerospace-grade-Carbon--Sigmatex--368gm%C2%B2-8HS-from-Germany
"kickthedonkey" has some of this for sale in Northern Germany ...
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search