I am developing a project with a wing included.
The wing core is balsa wood and I need to increase stiffness area. 
I think to reinforce with carbon fiber. Over this material I will paste several solar cells.
I milled a wing profile in foam with a 3D router milling.
I think to use your mould kit to create a mould and I will make carbon fiber process according your <<Carbon mods>> videos.

What do you think about this procedure?
mhdghoul
mhdghoul
Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)
Group: Forum Members
Posts: 49, Visits: 113
i guess since nobody answered your question , u have to try it to know , why dont u pm matt the admin he will surely answer u.

best regards mhd alghoul mhdghoul@hotmail.com youtube channel :atmospherejo link is http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Racing Mike
Racing Mike
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Awaiting Activation
Posts: 2, Visits: 17
Hi Marak,
I may be able to help. I produce carbon wings for model team racers.
What is the shape of your wing ? how long? how wide at root? and tip.
My wings are made in a alloy mould. I use a Rohacell core and carbon skins.
Here is a couple of pictures of what I make.

Mike



 http://www.talkcomposites.com/Uploads/Images/a8789da3-28c4-47a0-8471-6855.jpg
Wabba
Wabba
Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)
Group: Forum Members
Posts: 21, Visits: 64
Wow...
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
i bet this is called serious work.

I could stare at that for hours.

Is it spread tow fabric or simply a paint scheme?

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search