Epoxy Paste/Filler - what's the filler material?


Author
Message
jamesw
jamesw
Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)
Group: Forum Members
Posts: 61, Visits: 558
Am looking to create a mill-able epoxy paste - I currently have to buy it in at high cost - but wondered if I could use a epoxy coating resin plus some sort of filler powder to replicate for test/non critical jobs. This paste is used for patterns - after undersize milling low density foam and then remachining after cure to form a high quality surface for coating.

The mixed uncured consistency is like that of pastry, and cures to form a 0.5kg/m3 density coating similar to that of body filler.

I think polyester filler uses talc - anyone know if this is likely to work in a similar way with epoxy resin?

Thanks all,
Reply
jamesw
jamesw
Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)
Group: Forum Members
Posts: 61, Visits: 558
Thanks Fred, cured some overnight with glass bubbles - certainly had the right consistency - will see how it mills today..
I know you can also get a plastic based micro balloon - wonder how that changes things?

Anyone know if there are problems with tool-life and dust creation issues with machining these glass microspheres?

james