Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Tube and Section
»
Max Temperature for Tube
Max Temperature for Tube
Post Reply
Like
3
Max Temperature for Tube
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Denis
Denis
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 1,
Visits: 6
Hello,
I am looking for tube to make cylinders for a stationery steam engine.
What is the maximum temperature that your tube will safely work at please ?
Do you have 3 inch diameter tube available please ?
Thanks
Denis
Reply
Like
3
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
There are epoxy resins that are designed for extreme heat and must be autoclaved.
Try a website called Dragon Plate they have all kinds of preformed carbon fiber shapes.
Fred
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
The only Data we hold shows a HDT of 70
°C So I certainly wouldnt be risking steam down them!!
Also the biggest tube we stock is
60.3mm ID Carbon Fibre Tube.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search