How are carbon motorcycle wheels made??


Author
Message
James66
James66
Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)
Group: Forum Members
Posts: 10, Visits: 99
Hi all

New on here, ive been thinking about 'How' for a while + thought this may be a good place to ask

Ive got a carbon dymag front wheel on my race bike + figure out how its made, the spokes are hollow, hub is magnesium + the visable surface is smooth + well presented

Anybody have any knowledge on how these are made?

Its not so i can try + foolishly make some its just a huge curiosity

cheers

James
Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Here's his site

http://www.c12cfd.co.uk/index.htm

It was him who first taught me composites and got me interested!