Hi!
Mi name is Alessandro and I'm writing from Italy... I'm new to the forum and to composites world...
After three months studying over the internet two days ago a made my first infusion, an exhaust stirrup for my bike.. an easy part but it came out very good (no pinholes.. no bag leaks..) and I'm really happy with it.
I want to thank the forum since a didn't know anything about composites and I found many important advices reading your posts.. Thank you!



Alessandro
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
ciao benvenuto!!
alebassa
alebassa
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 48, Visits: 171
Grazie, ciao a te! Io sono vicino a Torino e tu?


Alessandro
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
Io sono dalla provincia di Treviso
alebassa
alebassa
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 48, Visits: 171
Posso chiederti se ti occupi di compositi per hobby o per lavoro? che tipo di parti fai??


Alessandro
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
per hobby, ho fatto un po' di parti per auto come pannelli porta, cruscottino ecc....
questo è il portamanometro con tutta la mascherina che mi son fatto per la mia auto.
Attachments
portaman-carbonio.JPG (588 views, 92.00 KB)
alebassa
alebassa
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 48, Visits: 171
ben fatto! Io sto iniziando a fare qualche pezzo per la mia moto, facendo gli stampi dai pezzi originali..

Per i materiali dove ti fornisici?


Alessandro
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
io li prendo a mestre da Angeloni...non fa vendita online però.
carbonrace
carbonrace
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 4, Visits: 23
Ciao !

Mi fa piacere vedere che ci sono altri italiani su questo forum che conoscono questo sito e i prodotti di easycomposites.
Ho fatto questo mestiere per diversi anni da titolare di azienda e ora eseguo alcuni manufatti ma solo per hobby;
sarei lieto di fornire la mia esperienza e le mie conoscenze se ne avrete bisogno.

Hi !

I'm glad to see that there are other Italians on this forum who know this site and products of easycomposites.
I've done this job for several years as owner of the company and now only as a hobby;
I would be happy to provide my experience and my knowledge if you need it
prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search