So I've decided to make my first project with carbon fiber a difficult one(not smart?). Ill post pictures as I progress and advice as to what I'm doing would be appreciated.

The idea is to make a mould that wraps around the edges as they can be seen while on the car.

The clay in the front of the light is to fill in the cosmetic groves that the carbon probably wont lay into, should I just fill them in with Gel-coat and sand them off the mould, or try to fill them in like I have now? The clay is hard to smooth out nice and ill probably have to sand anyway.

I would like to make this a repeatable process because I'm practicing on a used pair of lights first and if it comes out good Id like to do mine.

prep for mould making so far






Reply
383
383
Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)Supreme Being (176 reputation)
Group: Forum Members
Posts: 28, Visits: 99
Overall a better part but those problem areas are still haunting me. So what are the tricks to flattening folds when dealing with uneven compound radii? Do I just try to "rub" across the fold to lay it down or do I need to pull on a different part of the fabric to "stretch" it out? 

Is there a adhesive I can use to "pin" the carbon down or is that pre-preg?

I think my next step is to make another mold with a HUGE flange so I can lay a large square piece of carbon to work with.

 








GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
383 - 13 Years Ago
mhdghoul - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
MAVERICK - 13 Years Ago
383 - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
Joe - 13 Years Ago
383 - 13 Years Ago
Joe - 13 Years Ago
383 - 13 Years Ago
Mr Rooty Tooty - 13 Years Ago
383 - 13 Years Ago
Joe - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
Dave - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
Joe - 13 Years Ago
383 - 13 Years Ago
Joe - 13 Years Ago
383 - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
383 - 13 Years Ago
batbyggare - 13 Years Ago
383 - 13 Years Ago
Warren - 13 Years Ago
Warren - 13 Years Ago
mhdghoul - 13 Years Ago
383 - 13 Years Ago
383 - 13 Years Ago
383 - 13 Years Ago
neilb - 13 Years Ago
Rootz - 13 Years Ago
mr_goat - 13 Years Ago
383 - 13 Years Ago
andygtt - 13 Years Ago
TomDesign - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search