None of our silicones or resins will operate at that temperature.
You would realistically need to be looking at some kind of ceramic shield to reduce heat transfer through conduction and some kind of reflective layer over it to reflect radiated heat.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|