Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Patching Plastic Suitcase
Patching Plastic Suitcase
Post Reply
Like
19
Patching Plastic Suitcase
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
igb
igb
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 12
I've just returned home from Washington to find an 8cm split in one of our rigid suitcases, presumably where a sharp-edged case was pushed against it in the plane or during handling. The case is made of some sort of vacuum-formed Polypropylene, about 1mm thick. It's not worth claiming on insurance: it's five years old, scuffed, and the hassle and no-claims issues make it a non-starter. However, it's worth spending twenty quid to keep it going.
I've reinforced laptop lids and other flat surfaces in the past using carbon-fibre sheet and Araldite, but this is a slightly curved surface and the case is slightly flexible. I think just running Araldite into the crack will fail, as the mating surface would be just the thickness of the plastic and the slight flexing in use would rapidly crack the adhesive.
So I'm guessing that if I bought some Kevlar braid, soaked it in epoxy resin and laid it along the crack on the inside of the case, then that would be reasonably strong?
Tags
kevlar
luggage
polypropylene
repair
Reply
Like
19
brasco
brasco
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
i have the PERFECT product--
never seen or heard of it anywhere else--
patch
i do autobody repairs and i want to try this on a plastic bumper soon.
CarbonFiberCreations
Reply
Like
17
Warren (Staff)
Warren (Staff)
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
A patch type repair is definitely the way to go. As a one off repair, our
CarbonFibre Rapid Repair Kit
has everything you need for that kind of repair.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
15
igb
igb
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 12
Yes, thank you, I've ordered the kit.
Poking around your videos, I've found the one in which repairs are being made to a kayak, and I can adapt the technique. But I have one problem: I'd like to be able to get a gloss surface on a slightly concave section, and the technique of stretching release film over the area obviously doesn't work for that? Is there a technique, or do I need to accept the surface will need to be sanded and re-coated?
Reply
Like
19
brasco
brasco
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
sweet!
CarbonFiberCreations
Reply
Like
14
Warren (Staff)
Warren (Staff)
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
As you can't stretch it, you just have to smooth it by hand so there are no creases in the release film.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
18
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
19
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search