jamesw
jamesw
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 558
Anyone tried this before? Have a look for: EZ~Spray® Silicone 20
For those of us making multiple parts, it looks really good...
Would be good to hear of anyone using it, and if EC would recommend it?
James
Reply
Like
5
Reply
compositepro
compositepro
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 22,
Visits: 65
Drew Diller (14/07/2013)
No I don't go on velocipede - first I'd heard of it actually.
I can give you a quick background on myself - when still in essentially unconfident teenager mode I flunked out of college twice, once software engineering then mechanical engineering. I fell into software engineering for a living and ten years later I want to do mechanical engineering, lol. Whoooooops.
I think if you mistook me for an employee I must be on the right track? I hope so. My most pressing hangup right now is making a tough, leak free, reusable bladder. I have the mold creation end of things more or less covered. I get prepreg at what appears to be a very fair price straight from Zoltek. The consolidation and compression bit is what I don't have down yet.
(Is it just me or do the QUOTE tags on this forum not work intuitively?)
Hi Drew
I was wondering as Argonaut actually use a company called ICE for all their carbon knowledge,was wondering if they were moving away from them as there are a lot more folks asking questions online now regards Bladder molding and seeming not to have got as far as you have.
I actually worked in the USA many years ago in the bicycle industry, back when composites were in their infancy ,but moved away from it when i got involved with a guy who was working for a big military aeroplane company in Burbank
Turns out he got me a job back in good old England as he was quite high up in the F1 teams as far as composites engineering went and we kind of went from there, spending time in F1 Defence you kind of develop things which companies outside those industries then patent claiming its NEW but again the birth of my daughter has brought a career change hence we set up a bicycle consultancy and manufacturing company in the UK
If you get stuck for anything drop me aline chief
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Anyone tried a reusable silicone vacuum bag?
jamesw
-
12 Years Ago
I'm going to try this out soon... it indeed looks like a great technique to make more parts
matthieutje65
-
12 Years Ago
Post up the results!
jamesw
-
12 Years Ago
I ordered Smooth-On's test batch ... for making inflation semi-bladders, instead of vac bags. For...
Drew Diller
-
12 Years Ago
I'm doing a test of this stuff combined with a polystyrene plug that I'm going to dissolve with...
Drew Diller
-
12 Years Ago
Thx for the info, keep us updated ;) I'll start soon, once my first parts come out of the mould,...
matthieutje65
-
12 Years Ago
Drew - what was this product name from Smooth-on? Thanks Jim
JaWillis
-
11 Years Ago
I had some real bonehead moments regarding the inflation neck - it was leaky, or it would tear out,...
Drew Diller
-
12 Years Ago
How far did sample go I want to make a mold for air filter cover?
capnez
-
12 Years Ago
Well, this silicone bladder test didn't go so well - my result had wall thicknesses that were too...
Drew Diller
-
12 Years Ago
drew thats the process we use in industry, i work in design of composite bicycles in fact 20 years...
compositepro
-
12 Years Ago
"Ps your not the guy who's experimenting at argonaut?" Hey, thanks for the advice compositepro! I...
Drew Diller
-
12 Years Ago
[quote][b]Drew Diller (14/07/2013)[/b][hr]"Ps your not the guy who's experimenting at argonaut?"...
compositepro
-
12 Years Ago
Hello Well you have knowledge that we would all like to learn from. Could you post some pictures and...
fgayford
-
12 Years Ago
No I don't go on velocipede - first I'd heard of it actually. I can give you a quick background on...
Drew Diller
-
12 Years Ago
[quote][b]Drew Diller (14/07/2013)[/b][hr]No I don't go on velocipede - first I'd heard of it...
compositepro
-
12 Years Ago
Funny, your words on the "claiming its NEW" end of things... I was involved in helping prototype...
Drew Diller
-
12 Years Ago
IME ive seen a fair few go down with an idea when a big company has steamrollered them ,morally its...
compositepro
-
12 Years Ago
IME = In My Experience? Yeah I know what you mean - funny thing, I had some guys do some handy man...
Drew Diller
-
12 Years Ago
IME yep In my experience Plasti dip is like a coating over here in the UK for putting nice...
compositepro
-
12 Years Ago
Wow that stuff is CHEAP, half the cost of latex! And available locally. I'll play around with it....
Drew Diller
-
12 Years Ago
The green stuff is EZ-Brush vac bag silicone - http://www.smooth-on.com/index.php?cPath=1340 You...
Drew Diller
-
11 Years Ago
Watching with interest! Please post up any success in you technique!
20_rc51_00
-
11 Years Ago
Drew, How did things turn out? Did you give latex a try?
20_rc51_00
-
9 Years Ago
@20_rc51_00 Yo. Sorry, I haven't posted here in a while. Haven't posted anywhere in a while...
Drew Diller
-
9 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search