Hi, I would like to know what would be the best product to repair a crack that was occurred along the blades edge of my ice hockey stick. I need something that is extremely hard setting that can with-stand frequent impacts while playing.

Hope someone can help!

Regards

Brien
Reply
bbloom
bbloom
Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)
Group: Forum Members
Posts: 2, Visits: 13
cheers for the reply guys

Here are some pics of the crack. Its only a small crack along the blade, but i know one more knock and the blade will snap completely. So want to fix this before that happens.  I believe the fracture is deep into the blade, as I can hear the fibers snapping when i apply a little pressure.

Thanks for your time

Brien






Attachments
stick 002.JPG (977 views, 2.00 MB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search